identify the following welding imperfection: bad restart porosity undercut underfill incomplete joint…

identify the following welding imperfection: bad restart porosity undercut underfill incomplete joint penetration overlap excessive reinforcement crater crack valley

identify the following welding imperfection: bad restart porosity undercut underfill incomplete joint penetration overlap excessive reinforcement crater crack valley

Answer

Brief Explanations:

The image shows a welding defect where there is a lack of proper restart in the welding process, with a visible disruption in the weld bead pattern. Bad restart is characterized by such irregularities when the welding process is interrupted and then resumed.

Answer:

A. Bad Restart